HomeHomeDiscussionsDiscussionsOil Refinery Co...Oil Refinery Co...Crude overhead system Crude overhead system ' s demister corrosion
Previous
 
Next
New Post
1/2/2011 9:00 PM
 
After few week of operation , we have noticed severe corrosion of Crude Column Reflux Drum Demister pad .I am suspecting corrosion due to chloride as during initial start up desalter was not in line. Wire mesh SS304 have become fragile and getting broken on samll twist. Temp.in the equipment remains 150 to 200 DegC, pressure is approx.2 Kg/Cm2 Thanks in advance Let me know the reasons please.
 
Previous
 
Next
HomeHomeDiscussionsDiscussionsOil Refinery Co...Oil Refinery Co...Crude overhead system Crude overhead system ' s demister corrosion


The Hendrix Group, Inc.  |  15823 N. Barkers Landing  |  Houston, Texas 77079  |  Phone: (281) 556-8774  |  Fax: (281) 870-0659