Stress Corrosion Cracking Fracture

Stress Corrosion Cracking Fracture Of A Carbon Steel Weld

stress corrosion cracking in carbon steel

Cleavage fracture surface of a carbon steel weld from an emergency relief valve pipe. Fracture was believed to be due to C0-CO2-h30 stress corrosion cracking. (~250X)