Hydrogen Embrittlement Crack In AISI 9623 Low Alloy Steel

Hydrogen embrittlement crack initiated by corrosion of a AISI 9623 alloy in downhole service. The microstructure is unetched, case hardened, quenched and tempered martensite at HRC 29. 2% Nital Etch, 50X