Solid Metal Embrittlement Induced Cracking

Solid Metal Embrittlement Induced Cracking

Viton B elastomer, explosive decompression

Brittle crack in a cadmium plated B7 bolt from solid metal induced embrittlement due to exposure to elevated temperatures.