"galvanic corrosion"
Question:
"I'm building a copper roof over a bay window on the north side of my house. I want to secure a copper sheet/shingles to galvanized steel. To avoid corrosion, what type of screws can I use? Steel,zinc-plated,black-finish,or stainless.Copper rivets or self-sealing stainless steel are definite possibilities also."
Answer:
I would use either copper or 304 stainless steel screws.