NOTICE

Forums are temporarily disabled while we are working on a new login procedure.

When migrating the old forums over to our new forums we were unable to retain the identity of the authors, so the old posts will show up as "anonymous". All NEW posts will show up credited to their authors. So please participate and share knowledge just as you have in the past.

You must log in if you are an existing user or register if you are a new user in order to contribute to the discussions.

Discussion Forums - The Hendrix Group
HomeHomeDiscussionsDiscussionsMaterial Select...Material Select...Carbon steel Vs Naval Brass weldingCarbon steel Vs Naval Brass welding
Previous
 
Next
New Post
11/20/2002 9:00 AM
 
I had specified for an exchnager (AEL type) Admiralty tubes, (for cooling water) Naval brass for tube sheet, and CS for Shell (Naphtha) will there be any problem with the tube sheet to shell joint (welding), or for tubesheet to tube joint expecting your reply regards, N.S.Babu
 
New Post
11/24/2002 9:00 AM
 
Sear Sir: Your stated alloy combinations for the exchanger have been used with success. However, we are more familiar with carbon steel tubesheets with a brass overlay. David Hendrix The Hendrix Group Inc.
 
New Post
11/25/2002 9:00 AM
 
Thank you for your reply, Nnyway i had also raised the same query to some of the experienced personnel inthe refinery field, they also told the same, welding is not a problem, but if we specify AEL type the tube sheet can be specified as brass clad or overlay, for simple and good welding or we can specify AES type so that we can avoid the weld itself. However we have to look into the cost of the claded material and the AES floating head. the cheaper one can be used. N S Babu.
 
Previous
 
Next
HomeHomeDiscussionsDiscussionsMaterial Select...Material Select...Carbon steel Vs Naval Brass weldingCarbon steel Vs Naval Brass welding


  

News

With a little delay, our Calculation of Ammonium Salt Deposition Temperatures...read more
Our sulfidic corrosion calculators are now available at hghouston.com/calcula...read more

Stay Current

Sign up for our quarterly newsletter

covering updates on corrosion

Sign Up