NOTICE

Forums are temporarily disabled while we are working on a new login procedure.

When migrating the old forums over to our new forums we were unable to retain the identity of the authors, so the old posts will show up as "anonymous". All NEW posts will show up credited to their authors. So please participate and share knowledge just as you have in the past.

You must log in if you are an existing user or register if you are a new user in order to contribute to the discussions.

Discussion Forums - The Hendrix Group
HomeHomeDiscussionsDiscussionsMaterial Select...Material Select...SHEATH MATERIAL FOR HEATER SKIN THERMOCOUPLE - RADIATIOSHEATH MATERIAL FOR HEATER SKIN THERMOCOUPLE - RADIATIO
Previous
 
Next
New Post
4/15/2003 9:00 AM
 
PLS ADVISE SUITABLE METTULURGY FOR FIRED HEATERS SKIN THERMOCOUPLES SHEATH INSTALLED TO MEASURE THE TUBE SKIN TEMPERATURE IN RADIATION ZONE THE TEMPERATURE IS EXPECTED TO BE 1000 deg C but the tube skin temperature is 600 deg C THE FUEL CONTAINS SOME AMOUNT OF SULPHUR/H2S METALLURGY TRIED FOR THIS APPLICATION IS SS 446 & INCONEL 625 ANY BETTER MATERIAL WHICH CAN GIVE US A LONGER LIFE OF ROUGHLY 3 YEARS. REGARDS
 
New Post
4/17/2003 9:00 AM
 
Dear Sir: You might consider Haynes Alloy HR-160. Hope this helps! David Hendrix The Hendrix Group Inc.
 
Previous
 
Next
HomeHomeDiscussionsDiscussionsMaterial Select...Material Select...SHEATH MATERIAL FOR HEATER SKIN THERMOCOUPLE - RADIATIOSHEATH MATERIAL FOR HEATER SKIN THERMOCOUPLE - RADIATIO


  

News

With a little delay, our Calculation of Ammonium Salt Deposition Temperatures...read more
Our sulfidic corrosion calculators are now available at hghouston.com/calcula...read more

Stay Current

Sign up for our quarterly newsletter

covering updates on corrosion

Sign Up