HomeHomeDiscussionsDiscussionsMaterial Select...Material Select...Heat treat of S.S. 316LHeat treat of S.S. 316L
Previous
 
Next
New Post
9/17/2006 9:00 AM
 
You should refer to ASME Section 2 part D %E2%80“ Nonmandatory Appendix %E2%80%9CA%E2%80%9D paragraph A-350. Good Luck Scott
 
New Post
9/21/2006 9:00 AM
 
thanx all all answer%60s are very usful . but in ASME UHA-44,table UHA-44 ,percent of elongation & Design temp. are input to considering stress relieve or not. but S.S. 316L isn%60t in this table .plz explain for me is it a special item?
 
New Post
9/23/2006 9:00 AM
 
ASME code calls for PWHT for materials of a certain thickness%E2%80™ or alloyed material that would be susceptible to forming a martensitic micro structure (high hardness microstructure). 316L is an austenitic stainless steel that doesn't go through phase changes when welded or heated (stays austenitic because of the high austenizing elements - Nickel); meaning it will not form a hard micro structure in the HAZ even if quenched. Austenitic stainless steel can be aged hardened or strain aged hardened by cold working or if at high temperatures for a long period. Generally if you want to weld on material that has been aged hardened you want to solution anneal the material prior because the stresses in the material are high enough that welding is almost impossible %E2%80“ cracking will occur. As I mentioned in a previous response, there is a debate on PWHT austenitic SS for service environment to reduce the chances of SCC. PWHT would be done in the range were the SS material will become sensitized (you will loose corrosion resistance) but stresses would be reduced. To stay with the ASME code, you may want to look at ASME Section 2 part D %E2%80“ Nonmandatory Appendix %E2%80%9CA%E2%80%9D paragraph A-350. Are you determining if you are required to heat treat a component (vessel heads) or to heat treat welds?? Good luck Scott
 
New Post
9/23/2006 9:00 AM
 
I would also like to add, for a vessel in "Leathal Service" does require PWHT if the vessel is fabricated with carbon steel or low alloy steel regardless of thickness. 316L would not fall uder this so shouldn't require PWHT because of the service. Refer to UW 2 ASME Sect. 8 div. 1 Good Luck Scott
 
New Post
10/1/2006 9:00 AM
 
U R right Scott UW-2 is for C.S. & low alloy steels.But my problem is%60nt Only PWHT. Stress relive for Head%60s also is a problem.
 
Previous
 
Next
HomeHomeDiscussionsDiscussionsMaterial Select...Material Select...Heat treat of S.S. 316LHeat treat of S.S. 316L


  

News

With a little delay, our Calculation of Ammonium Salt Deposition Temperatures...read more
Our sulfidic corrosion calculators are now available at hghouston.com/calcula...read more

Stay Current

Sign up for our quarterly newsletter

covering updates on corrosion

Sign Up