NOTICE

Forums are temporarily disabled while we are working on a new login procedure.

When migrating the old forums over to our new forums we were unable to retain the identity of the authors, so the old posts will show up as "anonymous". All NEW posts will show up credited to their authors. So please participate and share knowledge just as you have in the past.

You must log in if you are an existing user or register if you are a new user in order to contribute to the discussions.

Discussion Forums - The Hendrix Group
HomeHomeDiscussionsDiscussionsGeneral Corrosi...General Corrosi...Stress corrosion of brassStress corrosion of brass
Previous
 
Next
New Post
8/14/2007 9:00 AM
 
I believe that if brass is used in compressive stress rather than tensile stress the propensity to suffer stress corrosion cracking is removed. Am I correct? Does anyone know of any learned papers that support this?
 
New Post
8/15/2007 9:00 AM
 
You can go thro' the topic in Hendrix Discussion Forum on Stress Corrosion Cracking in Brass which very categorically mentions that Stress corrosion cracking or "season cracking" occurs only in the simultaneous presence of a sufficiently high tensile stress and a specific corrosive environment like amoniacal or amines. But whether under compressive loading the intensity of SCC is removed is to be experimented under lab Simulators. regards
 
New Post
8/15/2007 9:00 AM
 
SCC to occur stress is also one factory.Simply by altering the type of stress you cant avoid SCC susceptibility material.Environment(medium)plays a major role even the amount of stress level is very low. SCC is a combination of MEDIUM INVOLVED STRESS INTENSITY LEVEL METHOD OF FABRICATION HEAT TREATMENT ETC. regards,
 
Previous
 
Next
HomeHomeDiscussionsDiscussionsGeneral Corrosi...General Corrosi...Stress corrosion of brassStress corrosion of brass


  

News

With a little delay, our Calculation of Ammonium Salt Deposition Temperatures...read more
Our sulfidic corrosion calculators are now available at hghouston.com/calcula...read more

Stay Current

Sign up for our quarterly newsletter

covering updates on corrosion

Sign Up