3/4/2010 9:00 AM
 
We all r using LPR probe in aq. Conductive phase like water to measure the running corrosion rate by it’s operating principle. But to my understanding the LPR projected corrosion rate reflects general corrosion rate and LPR probe cant discriminate between General and Pitting Corrosion rate. AM I CORRECT ? If I am correct – does anybody has any operating experience giving any alternate solutions like integrating ECN ( electrochemical noise) probe with LPR which can categorically identify pitting index/ corrosion due to DO or otherwise. Pl. share
 
New Post
3/15/2010 9:00 AM
 
We have LPR probes on tower water systems which mesure general corrosion and also pitting tendency. lm
 
New Post
3/15/2010 9:00 AM
 
dear lima, (1) can u provide me the make, model, capacity , span of the type of LPR u have used ? (2) Are u measuring pitting tendency by simple LPR probe by qualitative current/voltage imbalance or u have attached any 3rd party gadget for quantitative pitting evaluation (3) what is ur opinion or experience on ECN inputs with LPR ? pl. regards
 
New Post
3/16/2010 9:00 AM
 
Please go to http://www.caproco.com/catalog/pdf/Probes-Instruments/Linear-Polarization-Resistance/Fixed/Fixed-LPR-Projecting-2-or-3-Element.pdf Regards luis
 
New Post
3/16/2010 9:00 AM
 
also go to http://www.lazenby.net/literature/RCS%209030%20Plus%20Instrument-R.pdf luis
 
Previous
 
Next
HomeHomeDiscussionsDiscussionsOil Refinery Co...Oil Refinery Co...LPR probe to identify Pitting Corrosion in Water StreamLPR probe to identify Pitting Corrosion in Water Stream


  

News

Our NACE region and acidic sour water calculator is now available. This ...read more
Our HTHA calculation is now available for registered users.  This applic...read more

Stay Current

Sign up for our quarterly newsletter

covering updates on corrosion

Sign Up