8/5/2004 9:00 AM
 
PWHT 
Does the pipe welding of SS321 to SS321 require PWHT? If not why?
 
New Post
8/5/2004 9:00 AM
 
Kumar: Typically, welding 321SS to itself does not require a PHWT as it is not a hardenable material and its composition minimizes sensitization based on migration of cbromium carbides to grain boundaries. David Hendrix The Hendrix Group Inc.
 
New Post
3/15/2005 9:00 AM
 
As SS 321 & SS 347 are stabilized grade, we generally recommend stabilisation treatment, i.e., heating to approx 900 C, holding for two hr followed by air cooiling
 
Previous
 
Next
HomeHomeDiscussionsDiscussionsOil Refinery Co...Oil Refinery Co...PWHTPWHT


  

News

With a little delay, our Calculation of Ammonium Salt Deposition Temperatures...read more
Our sulfidic corrosion calculators are now available at hghouston.com/calcula...read more

Stay Current

Sign up for our quarterly newsletter

covering updates on corrosion

Sign Up